ʻO ka hui INCOLOY® 800H/800HT UNS N08810/UNS N08811

Wehewehe Pōkole:

ʻOi aku ka ikaika o ke kolo a me ka haki ʻana o nā huila INCOLOY 800H a me 800HT ma mua o ka huila INCOLOY 800. Aneane like nā palena hoʻohui kemika o nā huila ʻekolu.


Nā kikoʻī huahana

Nā Lepili Huahana

Ka Hoʻohui Kemika

ʻO ke kinikini mea C Si Mn S Cu Ni Cr Al Ti Fe ʻAl+Ti

ʻO Incoloy800H/HT

Min 0.05         30.0 19.0 0.15 0.15 39.0 0.30
Max 0.10 1.0 1.5 0.05 0.75 35.0 23.0 0.60 0.60   1.20
Manaʻo ʻO Incoloy 800HT:C:0.06~0.10,Al+Ti:0.85~1.20.

Nā Waiwai Mekanika

Kūlana ʻo Aolly

Ikaika tensile

Rm MpaMin

Ikaika hāʻawi

RP 0.2 Mpa Min

Hoʻolōʻihi

He 5%Min

hoʻomehana ʻia

448

172

30

Nā Waiwai Kino

Ka nui o ka paʻag/cm3

Kiko Heheʻe

7.94

1357~1385

Kūlana Maʻamau

Koʻokoʻo, Pā, Uea a me ka Waihona Hana- ASTM B 408 & ASME SB 408 (Rod & Bar), ASTM B 564 & ASME SB 564 (Forgings)

Pā, Pepa a me ka ʻĀpana -ASTM A240/A 480 & ASME SA 240/SA 480 (Papa, Pepa, a me ke Kaha), ASTM B 409/B906 & ASME SB 409/SB 906 (Papa, Pepa, a me ke Kaha)

Paipu a me ka Tube- ASTM B 407/B829 & ASME SB 407/SB 829 (Paipu a me nā Paipu Seamless), ASTM B 514/B 775 & ASME SB 514/SB 775 (Paipu Welded), ASTM B 515/B 751 & ASME SB 515/SB 751 (Paipu Welded)

Nā ʻAno Huahana ʻē aʻe -ASTM B 366/ASME SB 366 (Nā Mea Hoʻohui)

Nā ʻano o Incoloy 800H/Incoloy 800HT

Nā Hale Hana Incoloy Kiʻekiʻe

● Ikaika wela kiʻekiʻe

● Ikaika haki kolo kiʻekiʻe

● Kūpaʻa i ka oxidation a me ka carburization i nā wahi mahana kiʻekiʻe

● Kū'ē maikaʻi i ka palaho i nā ʻano ʻakika he nui

● Kū'ē maikaʻi i nā lewa he nui i loaʻa ka sulfur


  • Ma mua:
  • Aʻe:

  • E kākau i kāu leka ma aneʻi a hoʻouna mai iā mākou

    Nā huahana pili

    • ʻO ka hui INCOLOY® 925 UNS N09925

      ʻO ka hui INCOLOY® 925 UNS N09925

      ʻO ka INCOLOY alloy 925 (UNS N09925) he alloy nickel-hao-chromium paʻakikī me nā hoʻohui o ka molybdenum, keleawe, titanium a me ka alumini. Ua hoʻolālā ʻia e hāʻawi i ka hui pū ʻana o ka ikaika kiʻekiʻe a me ke kūpaʻa maikaʻi loa i ka pala. Ua lawa ka nui o ka nickel no ka pale ʻana i ka haki ʻana o ka chloride-ion stress corrosion. ʻO ka nickel, me ka molybdenum a me ke keleawe, hāʻawi pū i ke kūpaʻa koʻikoʻi i ka hōʻemi ʻana i nā kemika. Kōkua ka molybdenum i ke kūpaʻa ʻana i ka pitting a me ka crevice corrosion. Hāʻawi ka nui o ka chromium alloy i ke kūpaʻa ʻana i nā wahi oxidizing. Hoʻoulu ka hoʻohui ʻana o ka titanium a me ka alumini i kahi hopena hoʻoikaika i ka wā o ka mālama wela.

    • ʻO ke kinikini INCOLOY® A286

      ʻO ke kinikini INCOLOY® A286

      ʻO ka INCOLOY alloy A-286 kahi alloy hao-nickel-chromium me nā hoʻohui o ka molybdenum a me ka titanium. Hiki ke paʻakikī i ka wā kahiko no nā waiwai mechanical kiʻekiʻe. Mālama ka alloy i ka ikaika maikaʻi a me ke kūpaʻa oxidation i nā mahana a hiki i kahi o 1300°F (700°C). He austenitic ka alloy i nā kūlana metallurgical āpau. ʻO ka ikaika kiʻekiʻe a me nā ʻano hana hana maikaʻi loa o ka INCOLOY alloy A-286 e hoʻolilo i ka alloy i mea pono no nā ʻāpana like ʻole o nā mokulele a me nā turbines kinoea ʻoihana. Hoʻohana ʻia hoʻi no nā noi hoʻopaʻa i nā ʻenekini kaʻa a me nā ʻāpana manifold i kau ʻia i nā pae kiʻekiʻe o ka wela a me ke kaumaha a ma ka ʻoihana aila a me ke kinoea ma waho.

    • ʻO ka hui INCOLOY® 254Mo/UNS S31254

      ʻO ka hui INCOLOY® 254Mo/UNS S31254

      ʻO ka pā kila kila 254 SMO, i ʻike ʻia hoʻi ʻo UNS S31254, ua hoʻomohala mua ʻia no ka hoʻohana ʻana i loko o ka wai kai a me nā wahi ʻē aʻe e halihali ana i ka chloride. Ua manaʻo ʻia kēia papa he kila kila austenitic kiʻekiʻe loa; Ua kapa pinepine ʻia ʻo UNS S31254 he papa "6% Moly" ma muli o ka nui o ka molybdenum; loaʻa i ka ʻohana 6% Moly ka hiki ke kū i nā mahana kiʻekiʻe a mālama i ka ikaika ma lalo o nā kūlana haʻalulu.

    • ʻO ka hui INCOlOY® 825 UNS N08825/W.Nr. 2.4858

      ʻO ka hui INCOlOY® 825 UNS N08825/W.Nr. 2.4858

      ʻO ka INCOLOY alloy 825 (UNS N08825) he nickel-iron-chromium alloy me nā hoʻohui o ka molybdenum, keleawe, a me ka titanium. Ua hoʻolālā ʻia e hāʻawi i ke kūʻē kūikawā i nā ʻano ʻino he nui. Ua lawa ka nui o ka nickel no ke kūʻē ʻana i ka chloride-ion stress-corrosion cracking. ʻO ka nickel me ka molybdenum a me ke keleawe, hāʻawi pū i ke kūʻē koʻikoʻi i nā ʻano ʻino e like me nā mea i loaʻa nā waikawa sulfuric a me phosphoric. Kōkua pū ka molybdenum i ke kūʻē ʻana i ka pitting a me ka crevice corrosion. Hāʻawi ka nui o ka chromium o ka alloy i ke kūʻē ʻana i nā ʻano mea oxidizing e like me ka nitric acid, nitrates a me ka paʻakai oxidizing. Hana ka hoʻohui titanium, me kahi mālama wela kūpono, e hoʻopaʻa i ka alloy e kūʻē i ka sensitization i ka inter granular corrosion.

    • ʻO ka hui INCOLOY® 800 UNS N08800

      ʻO ka hui INCOLOY® 800 UNS N08800

      ʻO ka INCOLOY alloy 800 (UNS N08800) kahi mea i hoʻohana nui ʻia no ke kūkulu ʻana i nā lako e pono ai ke kūpaʻa i ka pala, ke kūpaʻa wela, ka ikaika, a me ke kūpaʻa no ka lawelawe a hiki i 1500°F (816°C). Hāʻawi ka Alloy 800 i ke kūpaʻa maʻamau i nā ʻano wai he nui a, ma muli o kona ʻano nickel, kūʻē i ka haki ʻana o ka palaho. I nā mahana kiʻekiʻe, hāʻawi ia i ke kūpaʻa i ka oxidation, carburization, a me ka sulfidation me ka haki a me ka ikaika kolo. No nā noi e pono ai ke kūpaʻa nui aʻe i ka haki a me ke kolo o ke kaumaha, ʻoi aku hoʻi ma nā mahana ma luna o 1500°F (816°C).