ʻO ke kinikini INCONEL® C-276 UNS N10276/W.Nr. 2.4819
| ʻO ke kinikini | mea | C | Si | Mn | S | P | Ni | Cr | Mo | W | Fe | Co | V |
| ʻO ke kinikiniC-276 | Min | 14.5 | 15.0 | 3.0 | 4.0 | ||||||||
| Max | 0.01 | 0.08 | 1.0 | 0.03 | 0.04 | Bkaulike | 16.5 | 17.0 | 4.15 | 7.0 | 2.50 | 0.35 |
| Kūlana ʻo Aolly | Ikaika tensile Rm Mpa Min | Ikaika hāʻawi RP 0.2Mpa Min | Hoʻolōʻihi He 5% Min |
| Shoʻonā | 690 | 283 | 45 |
| Ka nui o ka paʻag/cm3 | Kiko Heheʻe℃ |
| 8.89 | 1325~1370 |
ʻO ke koʻokoʻo, ka pā, ka uea a me ka waihona hana hao -ASTM B 462 (Rod, Bar a me Forging Stock), ASTM B 564 &,ASTM B 574 (uea)
Pā, Pepa a me ka ʻĀpana- ASTM B 575/B 906 & ASME SB 575/SB 906
Paipu a me ka Tube -ASTM B 622/B 829 & ASME SB 622/SB 829 (Paipu Seamless), ASTM B 626/B 751 & ASME SB 626/SB751 (Paipu Welded), ASTM B 619/B 775
Nā Huahana Kuʻihao -ʻO ka metala hoʻopihapiha INCONEL C-276 - AWS A5.14 / ERNiCrMo-4.
Ke kūpaʻa oxidation maikaʻi loa a hiki i ka makahiki 2000° F
● Kūpaʻa i ka carburization a me ka nitriding
● Ikaika maikaʻi loa i ka mahana kiʻekiʻe
● Kū'ē maikaʻi i ka haki ʻana o ka chloride stress-corrosion